Comparison of typical properties of hardened mortar NESTOR P0/4 with lime plaster

Parameter

measurement unit

NESTOR P0/4

lime plaster

method

compressive strength after 28 days

MPa

10,5

0

ČSN EN 1015-11

tensile strength after 28 days

MPa

2,2

0,4

ČSN EN 1015-11

bulk density

kg/m3

1505

1490